Fabrication of Sn and SnO2 Nanopowders by Low-Temperature Phase Transformation Method
Skip Navigation
Skip to contents

Journal of Powder Materials : Journal of Powder Materials

OPEN ACCESS
SEARCH
Search

Articles

Page Path
HOME > J Korean Powder Metall Inst > Volume 13(1); 2006 > Article
저온상변태법을 이용한 주석 및 산화주석 나노말의 제조
이근재, 주연준, 소용대, 김남훈, 이재성, 좌용호
Fabrication of Sn and SnO2 Nanopowders by Low-Temperature Phase Transformation Method
Kun-Jae Lee, Yeon-Jun Joo, Yong-Dae So, Nam-Hoon Kim, Jai-Sung Lee, Yong-Ho Choa
Journal of Korean Powder Metallurgy Institute 2006;13(1):46-51
DOI: https://doi.org/10.4150/KPMI.2006.13.1.046
1한양대학교 정밀화학공학과
2㈜나마텍
3㈜나마텍
4㈜대하 맨텍
5한양대학교 금속재료공학과
6한양대학교 정밀화학공학과
1Department of Fine Chemical Engineering, Hanyang University
2NAMATECH Co., Ltd Hanayang Business Incubator
3NAMATECH Co., Ltd Hanayang Business Incubator
4DaeHa ManTech Co., Ltd., Banwol Industrial Complex
5Department of Metallurgy and Materials Science, Hanyang University
6Department of Fine Chemical Engineering, Hanyang University
  • 26 Views
  • 0 Download
  • 0 Crossref
  • 0 Scopus

Through the volume change of Sn in a low-temperature phase transformation, the Sn nanopowder with high, purity, was fabricated by an economic and eco-friendly process. The fine cracks were spontaneously generated. in, Sn ingot, which was reduced to powders in the repetition of phase transformation. The Sn nanopowder with 50 run in size was obtained by the 24th repetitions of phase transformation by low-temperature and ultrasonic treatments. Also, the SnO_2 powder was fabricated by the oxidation of the produced Sn powder to the ingot and milled by the ultrasonic milling method. The SnO_2 nanopowder of 20 nm in size was fabricated after the milling for 180 h.